Elektroda Tangan 490Mpa Kanggo Baja Kekuwatan Dhuwur
Aplikasi & Standar & Cathetan:
1. Cocog kanggo welding baja karbon lan baja paduan rendah, uga karo kekuatan boiler, pipa, kendaraan, BANGUNAN, BRIDGE lan STRUKTUR liyane, kayata Q345.
2. Standar sing kita temoni: GB/T5117 E501, AWS A5.1 E701 & A5.1M E491, ISO2560-A:E 42 3 B 2 2, ISO 2560-B: E4915 A
Titik kanggo manungsa waé:
1. Sadurunge welding, elektroda kudu dipanggang ing 350 ℃ kanggo 1 jam lan dijupuk minangka needed.
2. Sadurunge welding, weldment kudu di resiki saka teyeng, lenga, banyu lan impurities liyane.
3. Welding kudu dileksanakake karo busur cendhak, welding pass sempit cocok."
Fitur
1. Low hidrogen kalium elektroda, stabil busur, ayu mbentuk, kepileh, sethitik cipratan, gampang de-slagging, resistance geni kulit apik, resistance porosity apik.
2. sifat mekanik meja, plastisitas sing apik, ketangguhan impact lan resistensi retak.
Elektroda tangan baja karbon rendah GEL-57, kelas internasional yaiku E7015, kelas China yaiku J507, kalebu elektroda alkalin natrium hidrogen rendah, cocok kanggo welding kekuatan kelas Q345 saka baja struktural campuran rendah.J minangka huruf wiwitan persimpangan baja struktural, sing tegese elektroda baja struktural.Kekuwatan tensile saka 50 logam lebur padha karo utawa luwih saka 490MPa (50 KGF/mm2).elektroda hidrogen natrium rendah.Elektroda ing baris karo model E5015, ngendi E nggantosi elektroda karo kekuatan tensile saka 50 logam nggabungke witjaksono utawa luwih saka 490MPa (50 KGF/mm2).1 nuduhake kabeh-posisi welding elektroda (welding flat, welding vertikal, welding horisontal, welding vertikal).elektroda hidrogen natrium rendah.Elektroda ora ngemot stabilizer busur lan mung bisa digunakake kanggo welding polaritas mbalikke DC.
Perusahaan & Pabrik
Komposisi produk lan sifat mekanik introduksi
KOMPONEN KIMIA:
ALLOY (wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | V |
ATURAN GB/T | 0.15 | 1.6 | 0.9 | 0.2 | 0.3 | 0.3 | 0.035 | 0.035 | 0.08 |
ATURAN AWS | 0.15 | 1.25 | 0.9 | 0.2 | 0.3 | 0.3 | 0.035 | 0.035 | 0.08 |
NILAI CONTOH | 0,075 | 1.17 | 0.5 | 0.04 | 0.02 | 0.007 | 0.017 | 0.009 | 0.01 |
PROPERTI MEKANIKAL:
PROPERTI | KEKUATAN PENGHASILAN (MPa) | KEKUATAN EXTENSION (MPa) | HEATTREAMENT ℃ xh | ELONGASI(%) | ||||||
ATURAN GB/T | 400 | 490 | AW | 20 | ||||||
ATURAN AWS | 400 | 490 | AW | 22 | ||||||
NILAI CONTOH | 460 | 555 | AW | 30 |
PARAMETER WELDING REKOMENDASI:
SPESIFIKASI DIAMETER (mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | |||||
LISTRIK | H/W | 80-110 | 100-130 | 130-180 | 180-230 | ||||
(Amp) | OW | 50-80 | 90-120 | 130-160 | - |
CATETAN:
H/W: pengelasan posisi horizontal
O/W: welding posisi over-head
Kasus Khas
Sertifikat
Komposisi produk lan sifat mekanik introduksi
KOMPONEN KIMIA:
ALLOY (wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | V |
ATURAN GB/T | 0.15 | 1.6 | 0.9 | 0.2 | 0.3 | 0.3 | 0.035 | 0.035 | 0.08 |
ATURAN AWS | 0.15 | 1.25 | 0.9 | 0.2 | 0.3 | 0.3 | 0.035 | 0.035 | 0.08 |
NILAI CONTOH | 0,075 | 1.17 | 0.5 | 0.04 | 0.02 | 0.007 | 0.017 | 0.009 | 0.01 |
PROPERTI MEKANIKAL:
PROPERTI | KEKUATAN PENGHASILAN (MPa) | KEKUATAN EXTENSION (MPa) | HEATTREAMENT ℃ xh | ELONGASI(%) | ||||||
ATURAN GB/T | 400 | 490 | AW | 20 | ||||||
ATURAN AWS | 400 | 490 | AW | 22 | ||||||
NILAI CONTOH | 460 | 555 | AW | 30 |
PARAMETER WELDING REKOMENDASI:
SPESIFIKASI DIAMETER (mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | |||||
LISTRIK | H/W | 80-110 | 100-130 | 130-180 | 180-230 | ||||
(Amp) | OW | 50-80 | 90-120 | 130-160 | - |
CATETAN:
H/W: pengelasan posisi horizontal
O/W: welding posisi over-head