Paduan nikel MIG ERNiCrMo-3 Soldering makings
KOMPONEN KIMIA:
ALLOY (wt%) | C | Mn | Si | Cr | Ni | Mo | Fe | Nb+Ta | P | S |
ATURAN GB/T | 0.10 | 0.50 | 0.50 | 20.0-23.0 | ≥58 | 8.0-10.0 | 5.0 | 3.0-4.2 | - | - |
ATURAN AWS | 0.10 | 0.50 | 0.50 | 20.0-23.0 | ≥58 | 8.0-10.0 | 5.0 | 3.15-4.15 | 0.02 | 0.02 |
NILAI CONTOH | 0.006 | 0.15 | 0.15 | 22.01 | 64.80 | 8.72 | 0.18 | 3.49 | 0.001 | 0.001 |
PROPERTI MEKANIKAL:
PROPERTI | KEKUATAN PENGHASILAN (MPa) | KEKUATAN EXTENSION (MPa) | NILAI IMPAK J/℃ | ELONGASI(%) | ||||
ATURAN GB/T | - | - | - | - | ||||
ATURAN AWS | - | - | - | - | ||||
NILAI CONTOH | - | 780 | 144/-196 | 45 |
Nikel-kromium-molybdenum nikel-base alloy gas welding wire, komposisi nominal punika 61% Ni-22% Cr-9% Mo-3.5% Nb + Ta.
Sifat mekanik sing apik lan tahan kanggo korosi pitting lan crevice saka logam molten.
Pakan kabel Gamelan, busur stabil, mbentuk ayu, aliran apik saka logam panas, kurang cipratan, karo kinerja proses welding banget.
-
China Global demethane Tower
-
Zhejiang Petrokimia diesel/tangki penyimpanan minyak mentah
-
300.000 ton Offshore Floating Production and Storage Tanker (FPSO)
KOMPONEN KIMIA:
ALLOY (wt%) | C | Mn | Si | Cr | Ni | Mo | Fe | Nb+Ta | P | S |
ATURAN GB/T | 0.10 | 0.50 | 0.50 | 20.0-23.0 | ≥58 | 8.0-10.0 | 5.0 | 3.0-4.2 | - | - |
ATURAN AWS | 0.10 | 0.50 | 0.50 | 20.0-23.0 | ≥58 | 8.0-10.0 | 5.0 | 3.15-4.15 | 0.02 | 0.02 |
NILAI CONTOH | 0.006 | 0.15 | 0.15 | 22.01 | 64.80 | 8.72 | 0.18 | 3.49 | 0.001 | 0.001 |
PROPERTI MEKANIKAL:
PROPERTI | KEKUATAN PENGHASILAN (MPa) | KEKUATAN EXTENSION (MPa) | NILAI IMPAK J/℃ | ELONGASI(%) | ||||
ATURAN GB/T | - | - | - | - | ||||
ATURAN AWS | - | - | - | - | ||||
NILAI CONTOH | - | 780 | 144/-196 | 45 |