Baja paduan rendah Elektroda manual E7016-B2L sambungan sambungan logam
Wesi wesi kurang hidrogen kalium jinis rod welding tangan, busur stabil
Kurang cipratan, cetakan apik, gampang mbusak slag kinerja X-Ray
Sifat mekanik sing stabil, ketangguhan dampak sing dhuwur bisa dijaga ing kahanan perawatan panas
KOMPONEN KIMIA:
ALLOY (wt%) | C | Si | Mn | P | S | Ni | Cr | Mo | Liyane |
ATURAN GB/T | 0.037 | 0.28 | 0.82 | 0.011 | 0.008 | 0.012 | 1.21 | 0.48 | - |
PROPERTI MEKANIKAL:
PROPERTI | KEKUATAN PENGHASILAN (MPa) | KEKUATAN EXTENSION (MPa) | Elongasi (%) | NILAI IMPAK J/℃ | Perlakuan panas °C*h | |||||
ATURAN GB/T | 480 | 575 | 24 | 170/suhu normal | 690*1 |
PARAMETER WELDING REKOMENDASI:
SPESIFIKASI DIAMETER (mm) | 3.2*350 | 4.0*400 | 5.0*400 | ||||
LISTRIK (Amp) | H/W | 90-130 | 140-190 | 190-240 | |||
O/W | 80-120 | 120-160 | - |
-
Mei Jin Hua Sheng
menara sintetik glikol
-
Hainan Huasheng
menara pemulihan fenol
-
GDS-2209/GXS-E330
situs las permukaan tabung
KOMPONEN KIMIA:
ALLOY (wt%) | C | Si | Mn | P | S | Ni | Cr | Mo | Liyane |
ATURAN GB/T | 0.037 | 0.28 | 0.82 | 0.011 | 0.008 | 0.012 | 1.21 | 0.48 | - |
PROPERTI MEKANIKAL:
PROPERTI | KEKUATAN PENGHASILAN (MPa) | KEKUATAN EXTENSION (MPa) | Elongasi (%) | NILAI IMPAK J/℃ | Perlakuan panas °C*h | |||||
ATURAN GB/T | 480 | 575 | 24 | 170/suhu normal | 690*1 |
PARAMETER WELDING REKOMENDASI:
SPESIFIKASI DIAMETER (mm) | 3.2*350 | 4.0*400 | 5.0*400 | ||||
LISTRIK (Amp) | H/W | 90-130 | 140-190 | 190-240 | |||
O/W | 80-120 | 120-160 | - |