Baja paduan rendah Flux cored wire E71T8-K6-J Soldering jointing
KOMPONEN KIMIA:
ALLOY (wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | Al |
ATURAN GB/T | 0.12 | 1.75 | 0.80 | - | 0.3-1.0 | 0.35 | 0.03 | 0.03 | 1.80 |
ATURAN AWS | 0.15 | 0,5-1,50 | 0.80 | 0.20 | 0.4-1.0 | 0.15 | 0.03 | 0.03 | 1.80 |
NILAI CONTOH | 0.05 | 1.20 | 0.1 | 0.01 | 0.95 | 0.01 | 0.01 | 0.010 | 1 |
PROPERTI MEKANIKAL:
PROPERTI | KEKUATAN PENGHASILAN (MPa) | KEKUATAN EXTENSION (MPa) | NILAI IMPAK J/℃ | ELONGASI(%) | Perlakuan panas°Cxh | |||||
ATURAN GB/T | 390 | 490-670 | 27/-40 | 18 | AW | |||||
ATURAN AWS | 400 | 490-620 | 47/-40 | 20 | AW | |||||
NILAI CONTOH | 475 | 565 | 150/-40 | 27 | AW |
PARAMETER WELDING REKOMENDASI:
SPESIFIKASI DIAMETER (mm) | 1.6 | 2.0 | ||||||
Volt | 15-20 | 15-20 | ||||||
Amp | 180-250 | 180-300 | ||||||
dawa ekstensi garing (mm) | 10-20 | 10-20 |
490MPa kelas alkalin dhewe nglindhungi flux-inti kabel.
Arc stabil, kurang cipratan, mbentuk ayu, aman slag apik, karo kinerja welding banget.
Wis kinerja impact suhu kurang apik.
-
China Reaktor hidrogenasi abot
-
Qinghai Youjian Wunan Oilfield
-
Proyek LNG-2 Arktik
KOMPONEN KIMIA:
ALLOY (wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | Al |
ATURAN GB/T | 0.12 | 1.75 | 0.80 | - | 0.3-1.0 | 0.35 | 0.03 | 0.03 | 1.80 |
ATURAN AWS | 0.15 | 0,5-1,50 | 0.80 | 0.20 | 0.4-1.0 | 0.15 | 0.03 | 0.03 | 1.80 |
NILAI CONTOH | 0.05 | 1.20 | 0.1 | 0.01 | 0.95 | 0.01 | 0.01 | 0.010 | 1 |
PROPERTI MEKANIKAL:
PROPERTI | KEKUATAN PENGHASILAN (MPa) | KEKUATAN EXTENSION (MPa) | NILAI IMPAK J/℃ | ELONGASI(%) | Perlakuan panas°Cxh | |||||
ATURAN GB/T | 390 | 490-670 | 27/-40 | 18 | AW | |||||
ATURAN AWS | 400 | 490-620 | 47/-40 | 20 | AW | |||||
NILAI CONTOH | 475 | 565 | 150/-40 | 27 | AW |
PARAMETER WELDING REKOMENDASI:
SPESIFIKASI DIAMETER (mm) | 1.6 | 2.0 | ||||||
Volt | 15-20 | 15-20 | ||||||
Amp | 180-250 | 180-300 | ||||||
dawa ekstensi garing (mm) | 10-20 | 10-20 |