CEHigh Carbon steels Elektroda manual E7018 aksesoris fabrikasi las
Aplikasi
Cocog kanggo welding saka baja karbon lan baja paduan rendah, uga karo kekuatan boiler, pipa, kendaraan, BANGUNAN, BRIDGE lan STRUKTUR liyane, kayata Q345.
Standar sing kita temoni: GB/T5117 E5018, AWS A5.1 E7018 & A5.1M E4918, ISO2560-A:E 42 3 B 3 2, ISO 2560-B: E4918 A.
KOMPONEN KIMIA:
ALLOY (wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | V |
ATURAN GB/T | 0.15 | 1.60 | 0.90 | 0.20 | 0.30 | 0.30 | 0.035 | 0.035 | 0.08 |
ATURAN AWS | 0.15 | 1.60 | 0.75 | 0.20 | 0.30 | 0.30 | 0.035 | 0.035 | 0.08 |
NILAI CONTOH | 0.071 | 1.28 | 0.45 | 0.02 | 0.01 | 0.04 | 0.017 | 0.008 | 0.01 |
PROPERTI MEKANIKAL:
PROPERTI | KEKUATAN PENGHASILAN (MPa) | KEKUATAN EXTENSION (MPa) | HEATTREAMENT ℃ xh | NILAI IMPAK J/℃ | ELONGASI(%) | ||||
ATURAN GB/T | 400 | 490 | AW | 27/-30 | 20 | ||||
ATURAN AWS | 400 | 490 | AW | 27/-30 | 22 | ||||
NILAI CONTOH | 495 | 590 | AW | 138/-30 | 27 |
PARAMETER WELDING REKOMENDASI:
SPESIFIKASI DIAMETER (mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | |||||
LISTRIK (Amp) | H/W | 80-110 | 110-130 | 130-180 | 180-230 | ||||
O/W | 50-80 | 90-120 | 130-160 | - |
Kekhasan
Wesi bubuk elektroda tangan jinis hidrogen rendah, efisiensi las sing dhuwur, busur stabil, pembentukan sing apik.
Corrugations, sethitik cipratan, gampang de-slagging, tamba apik resistance geni kulit, resistance stotal apik.
Sifat mekanik sing stabil, plastisitas sing apik lan ketekunan impact suhu sing kurang.
Nuduhake rincian
Stabilitas arc
wangun ayu
Babagan kita
Pabrik fioor tampilan
Kasus aplikasi
8,2-ton akeh operator
Reaktor internal
shooting pabrik nyata
KOMPONEN KIMIA:
ALLOY (wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | V |
ATURAN GB/T | 0.15 | 1.60 | 0.90 | 0.20 | 0.30 | 0.30 | 0.035 | 0.035 | 0.08 |
ATURAN AWS | 0.15 | 1.60 | 0.75 | 0.20 | 0.30 | 0.30 | 0.035 | 0.035 | 0.08 |
NILAI CONTOH | 0.071 | 1.28 | 0.45 | 0.02 | 0.01 | 0.04 | 0.017 | 0.008 | 0.01 |
PROPERTI MEKANIKAL:
PROPERTI | KEKUATAN PENGHASILAN (MPa) | KEKUATAN EXTENSION (MPa) | HEATTREAMENT ℃ xh | NILAI IMPAK J/℃ | ELONGASI(%) | ||||
ATURAN GB/T | 400 | 490 | AW | 27/-30 | 20 | ||||
ATURAN AWS | 400 | 490 | AW | 27/-30 | 22 | ||||
NILAI CONTOH | 495 | 590 | AW | 138/-30 | 27 |
PARAMETER WELDING REKOMENDASI:
SPESIFIKASI DIAMETER (mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | |||||
LISTRIK (Amp) | H/W | 80-110 | 110-130 | 130-180 | 180-230 | ||||
O/W | 50-80 | 90-120 | 130-160 | - |