AWS E8015-B1 Baja paduan rendah Elektroda manual Barang pengelasan
Aplikasi & Standar & Cathetan:
GER-207 rod welding tangan baja tahan panas (R207) 0,5% Cr-0,5% Mo rod welding tangan baja cocok kanggo welding CrMo pearlite baja tahan panas lan suhu dhuwur, pipa tekanan dhuwur, wadhah kimia lan baja liyane sing cocog, kayata 12CrMo piring tabung, tabung A335-P2, piring A387Gr.2. Kondisi welding: preheating lan saluran (lapisan) suhu: 160 ~ 190 ℃; 3. Perawatan panas: 690 ± 15 ℃ x 1h perawatan panas ditindakake miturut syarat standar bahan welding.
AWS E8015-B1 jinis elektroda tangan kanggo baja tahan panas cocok kanggo welding CrMo pearlite baja tahan panas (kayata 12CrMo, etc.) lan suhu dhuwur, pipa tekanan dhuwur, wadhah kimia lan baja cocog liyane. Sadurunge welding, elektroda kudu dipanggang ing bab 350 ℃ kanggo 1h, lan banjur digunakake karo baking. Sadurunge welding, weldment kudu di resiki saka teyeng, lenga, banyu lan impurities liyane.
Fitur
AWS E8015-B1 (R207) jinis tangan welding elektroda kanggo panas baja tahan punika sodium hidrogen jinis elektroda tangan welding kurang, busur stabil, kurang cipratan, mbentuk apik, desagging gampang, kinerja X-Ray banget. Elektroda las tangan digunakake akeh ing tenaga listrik, teknik tenaga, petrokimia lan industri liyane, sing paling umum digunakake Cr-Moh lan Mn-Mo jinis baja tahan panas lan Cr-Mo basis multi-elemen baja tahan panas. Sampeyan uga perlu kanggo nggunakake cara preheating sadurunge welding posisi lan welding formal kanggo welding baja tahan panas. Yen weldment kuwat, iku kudu preheated minangka kabèh. Sawise welding, weldment kudu katahan ing ndhuwur suhu preheating kanggo sawetara jam, lan banjur alon digawe adhem.
Perusahaan & Pabrik
Komposisi produk lan sifat mekanik introduksi
Komposisi produk lan sifat mekanik introduksi
KOMPONEN KIMIA:
ALLOY (wt%) | C | Mn | Si | Cr | Mo | P | S |
ATURAN GB/T | 0.05-0.12 | 0.90 | 0.80 | 0.40-0.65 | 0.40-0.65 | 0.03 | 0.030 |
ATURAN AWS | 0.05-0.12 | 0.90 | 0.80 | 0.40-0.65 | 0.40-0.65 | 0.03 | 0.030 |
NILAI CONTOH | 0,078 | 0.72 | 0.35 | 0.56 | 0.53 | 0.016 | 0.01 |
PROPERTI MEKANIKAL:
PROPERTI | KEKUATAN PENGHASILAN (MPa) | KEKUATAN EXTENSION (MPa) | HEATTREAMENT ℃ xh | NILAI IMPAK J/℃ | ELONGASI(%) | |||||||||
ATURAN GB/T | 460 | 550 | 690*1 | - | 17 | |||||||||
ATURAN AWS | 460 | 550 | 690*1 | - | 19 | |||||||||
NILAI CONTOH | 490 | 590 | 690*1 | 90/suhu normal | 23 |
PARAMETER WELDING REKOMENDASI:
SPESIFIKASI DIAMETER (mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | ||||||
LISTRIK (Amp) | H/W | 80-110 | 100-130 | 130-180 | 170-210 | |||||
O/W | 60-100 | 80-120 | 120-160 | - |
DETAIL PACKING:
SEPCIFIKASI | LENGKA | PCS / 1KG | BOOT / 1KG | |||
2,6 mm | 300 mm | 48PCS | 2KG | |||
3,2 mm | 350 mm | 27 PCS | 5kg | |||
4,0 mm | 350 mm | 16PCS | 5kg | |||
5,0 mm | 350 mm | 12 PCS | 5kg |
Kasus Khas
Sertifikat
Komposisi produk lan sifat mekanik introduksi
KOMPONEN KIMIA:
ALLOY (wt%) | C | Mn | Si | Cr | Mo | P | S |
ATURAN GB/T | 0.05-0.12 | 0.90 | 0.80 | 0.40-0.65 | 0.40-0.65 | 0.03 | 0.030 |
ATURAN AWS | 0.05-0.12 | 0.90 | 0.80 | 0.40-0.65 | 0.40-0.65 | 0.03 | 0.030 |
NILAI CONTOH | 0,078 | 0.72 | 0.35 | 0.56 | 0.53 | 0.016 | 0.01 |
PROPERTI MEKANIKAL:
PROPERTI | KEKUATAN PENGHASILAN (MPa) | KEKUATAN EXTENSION (MPa) | HEATTREAMENT ℃ xh | NILAI IMPAK J/℃ | ELONGASI(%) | |||||||||
ATURAN GB/T | 460 | 550 | 690*1 | - | 17 | |||||||||
ATURAN AWS | 460 | 550 | 690*1 | - | 19 | |||||||||
NILAI CONTOH | 490 | 590 | 690*1 | 90/suhu normal | 23 |
PARAMETER WELDING REKOMENDASI:
SPESIFIKASI DIAMETER (mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | ||||||
LISTRIK (Amp) | H/W | 80-110 | 100-130 | 130-180 | 170-210 | |||||
O/W | 60-100 | 80-120 | 120-160 | - |
DETAIL PACKING:
SEPCIFIKASI | LENGKA | PCS / 1KG | BOOT / 1KG | |||
2,6 mm | 300 mm | 48PCS | 2KG | |||
3,2 mm | 350 mm | 27 PCS | 5kg | |||
4,0 mm | 350 mm | 16PCS | 5kg | |||